Regarding the thin-ness of the 'paint' on the dials, could they be electroplating with certain salt solutions?
That would achieve as 'thin' a coating or many different hues as you like, according to the current / exposure time / salt recipe.
Regards,
MTF
Hirota-san, I am not......
By: MTF : October 4th, 2011-21:10
Hirota-san, I appreciate your explanations and await further knowledge. Unfortunately, I am not the famous Dr Thomas Mao But we may have met before, when I was a 'salaryman' in Tokyo: 2000 - 2001 and 2004 - 2006. Regards, MTF This message has been edited ...
Supplement
By: HIROTA, Masayuki : October 4th, 2011-23:28
Covering lacquer has been thought to be better to have flatter surface. But Patek try to give relatively rough surface (looks sand blasted) on covering lacquer. The dial seems glossy if you see it squarely. But from an angle, you will notice that the surf...